Hogar Blog

Waterborne Epoxy Hardener: The Cost Behind the VOC Label

Waterborne Epoxy Hardener: The Cost Behind the VOC Label
November 27, 2026

Waterborne epoxy hardener is an amine adduct carried in water instead of solvent. Across the 14 YLH-W grades, AHEW spans 73-300 g/eq, so the hardener mass at a fixed 100 µm film moves from 32 to 70 g/m2. Dosing from the amine value instead under-doses by up to 82%. Water costs dwell time, not money.

Glass jar of hazy pale waterborne amine hardener beside a beaker of clear water on a stainless bench

Figure 1. A waterborne amine hardener is a hazy liquid; the beaker beside it is the whole solvent load.

1. Introduction

Water is excluded from the VOC figure by definition, so a waterborne coating sells as low-VOC while still carrying an amine. The hardener is part of that package, and the part most often dosed from the wrong number.

Fourteen grades sit in the YLH-W range, from AHEW 73 g/eq to 300 g/eq. Every figure comes from the 2026 Yolatech catalog and its product pages.

2. Materials and Methods: What the Waterborne Epoxy Hardener Range Covers

The YLH-W series is a set of waterborne amine hardeners, supplied as aqueous adducts for two-pack systems where water is the only carrier.

2.1 Product identification and specification

Table 1 lists the range as printed on catalog page 14; AHEW spreads over a factor of four.

Table 1. Waterborne amine hardeners, YLH-W series, from the 2026 Yolatech catalog, page 14.

Grade

AHEW, g/eq

Amine value, mg KOH/g

Viscosity, mPa·s

phr

Pot life, min

YLH-1002W

284

150-190

8,000-12,000

145

60

YLH-1003W

300

150-190

25,000-45,000

140-180

60

YLH-1005W

120

250-300

6,000-13,000

60

60-120

YLH-1006W

151

185-225

12,000-25,000

77

90

YLH-1007W

73

380-420

80,000-150,000

35-40

120

YLH-1008W

240

150-180

100-400

125

70

YLH-1009W

145

200-230

23,000-31,000

75

30

YLH-1011W

145

250-280

3,500-5,500

70-80

40

YLH-1013W

150

240-280

5,000-10,000

77

35

YLH-1014W

170

200-250

500-1,300

87

60

YLH-1501W

285

100-200

5,000-20,000

115-120

not stated

YLH-2001W

300

140-180

8,000-15,000

150

not stated

YLH-2003W

96

300-360

1,000-1,500

50

65

YLH-3001W

150

280-320

8,000-25,000

75-80

not stated

No product page is live for these grades, so the catalog is the source; the resin side sits on the solid bisphenol A epoxy resin and liquid bisphenol A epoxy resin pages.

2.2 Test methods and data sources

The catalog does not name its methods. The figures correspond to: EEW according to ASTM D1652 or ISO 3001, amine value according to ISO 9702, viscosity measured at 25 °C by ASTM D445.

Pot life carries no test temperature or film thickness; an "18h" suffix on one aromatic grade of the same page fixes the default unit as minutes. Two entries need a note: YLH-1008W is printed at 400-100 mPa·s, read here as an inverted range, and YLH-1501W does not sit on the same phr basis. No duplicate runs are reported.

3. Results and Discussion: Amine Value, AHEW and Dosage

One number divides the fourteen grades: AHEW. It sets phr, and phr sets hardener mass per square metre.

3.1 Why the amine value cannot be converted into AHEW

If every amine group were primary, AHEW would follow 28,050 divided by the amine value. Nine grades break that relation, all in the same direction.

Table 2. Amine value converted to AHEW on an all-primary assumption, against the catalog AHEW.

Grade

Amine value, midpoint

AHEW if all primary

Catalog AHEW

Gap

YLH-1007W

400

70

73

+4%

YLH-1006W

205

137

151

+10%

YLH-2003W

330

85

96

+13%

YLH-1005W

275

102

120

+18%

YLH-1014W

225

125

170

+36%

YLH-1013W

260

108

150

+39%

YLH-1008W

165

170

240

+41%

YLH-1002W

170

165

284

+72%

YLH-1003W

170

165

300

+82%

The gap is the neutralised tertiary amine: the acid salt makes the adduct dispersible, that nitrogen titrates as amine value, and it never opens an oxirane ring.

Dosing from the amine value under-charges the system, by 4% on YLH-1007W and 82% on YLH-1003W. Ask for AHEW on the certificate, not the amine value.

3.2 Waterborne amine against a solvent-borne polyamide

The YLH-5022 polyamide is the reference solvent-borne option: 95% solids minimum, AHEW 165-185 g/eq, 30,000-80,000 cps at 25 °C, and xylene for viscosity.

Table 3. Waterborne amine YLH-1005W against the solvent-borne polyamide YLH-5022, at resin EEW 190.

Property

Waterborne amine YLH-1005W

Solvent-borne polyamide YLH-5022

Carrier

water

none, user adds xylene

AHEW, g/eq

120

165-185

phr at EEW 190

63

87-97

Viscosity at 25 °C

6,000-13,000 mPa·s

30,000-80,000 cps

Non-volatile, %

not published

95 minimum

Pot life

60-120 min

not published

Contribution to VOC

water excluded, acid counts

solvent is the VOC

Damp concrete

YLH-1003W is the damp grade

not recommended

Neither wins outright. The polyamide buys a wide application window and pays in solvent; the waterborne grade pays in dwell time.

4. Formulation and Dosage Calculation

Dosage follows one line: phr = 100 × AHEW ÷ EEW. At EEW 190, AHEW 120 gives 63 phr and AHEW 300 gives 158 phr.

Table 4. Hardener dosage and mass per square metre at 100 µm dry film, resin EEW 190, cured density 1.15 g/cm3.

AHEW, g/eq

phr

Binder, g/m2

Hardener mass, g/m2

73

38.4

115

31.9

120

63.2

115

44.5

240

126.3

115

64.2

300

157.9

115

70.3

That is a 2.2-fold spread in the second-most expensive component of the paint: about USD 0.15/m2 at an illustrative USD 4/kg.

Water adds a cost that never reaches the invoice. Removing 94 g/m2 of water takes 244 kJ/m2; 49 g/m2 of xylene takes 27 kJ/m2.

Table 5. Volatile removal at 100 µm dry film, model systems at 55% and 70% weight solids.

Item

Waterborne, 55% solids

Solvent-borne, 70% solids

Wet coating, g/m2

209

164

Volatile to remove, g/m2

94

49

Heat, kJ/kg

2,591

541

Heat, kJ/m2

244

27

Dwell at 1.5 kW/m2, s

163

18

Heat is cheap and dwell time is not: at a 1.5 kW/m2 flux the water film needs 163 s against 18 s, which is oven length, not a utility bill. On an air-drying line, the penalty is usually a longer recoat interval.

5. Processing Notes and Operating Window

Three settings decide whether a waterborne amine cures properly: induction time, humidity and wet film thickness. All three are shop variables.

• Induction: 5-10 minutes of standing after mixing lets the dispersion wet out and air escape. Skip it and the film typically shows pinholes.

• Humidity: above 85% RH the water cannot leave fast enough and the amine reacts with CO2 at the surface. White bloom follows within hours.

• Substrate: 10 °C minimum and 3 °C above the dew point. A cold slab pulls moisture from the air and the film never clarifies.

• Cure reading: the film clears as water leaves, but clearing is not cure. A 30-minute pot life turns a 20 kg kit into a 5 kg one.

Worker rolling milky white waterborne epoxy onto a concrete floor, half the floor cured clear

Figure 2. The wet edge stays milky white and the cured strip behind it goes clear; judging dryness at the wet edge is how second coats get locked in.

6. Applications: Where Each Waterborne Epoxy Hardener Earns Its Place

Four application families account for most of the range, each leaning on a different property.

6.1 Concrete floors, including damp slabs

YLH-1003W is the grade listed for damp surfaces, at 140-180 phr and 60 minutes pot life; YLH-1008W is the non-ionic grade for penetration at 125 phr. Dosage sits high because the slab absorbs water and binder alike; a slab above the project moisture limit fails under any hardener.

6.2 Steel protection and shop primers

YLH-1005W is the non-sagging grade at 60 phr, YLH-1006W the hardness grade at 77 phr, YLH-1011W the impact grade at 70-80 phr. Flash rust on blasted steel is the failure point, and a damp shop closes the window.

6.3 Gloss topcoats for wood and architectural panels

YLH-1009W gives high gloss and fast drying at 75 phr with 30 minutes of pot life; YLH-1013W trades speed for chemical resistance at 77 phr. Batch size follows pot life, not convenience.

6.4 Adhesives and cementitious primers

YLH-2003W is the water-soluble grade at 96 g/eq and 50 phr; YLH-3001W brings flexibility and salt spray resistance at 75-80 phr. Porous substrates starve the bond line by absorbing water. The YLH-3023 cycloaliphatic amine is the solvent-borne comparator.

Table 6. Application map for the waterborne amine range.

Application

Grade

Dosage, phr

Function

Failure point

Concrete floor

YLH-1003W

140-180

adhesion on damp slab

rising moisture

Steel primer

YLH-1005W

60

non-sagging film

flash rust

Gloss topcoat

YLH-1009W

75

gloss and fast set

30 min pot life

Cementitious primer

YLH-3001W

75-80

flexibility, salt spray

absorption by substrate

Damp concrete floor with water sheen meeting the wet edge of a milky waterborne epoxy coating

Figure 3. A damp slab is workable and standing water is not; the wet edge in this photograph is the limit, not the target.

7. Limitations and Material Verification

Four gaps limit what this dataset can support.

7.1 Known limitations and out-of-scope cases

The range covers hardeners only. No waterborne epoxy dispersion is published, so the resin side comes from a solid grade such as the solution-type bisphenol A epoxy resin, and dispersing is a separate step.

Non-volatile content is not printed for any W grade, so VOC per litre cannot be computed from the catalog alone. Salt spray remarks on page 14 are qualitative, with no hours and no data.

YLH-1501W sits off-basis: its phr of 115-120 implies a resin EEW of 243 g/eq, while the other thirteen cluster at 187-200. The range is also wrong for neat casting.

7.2 Incoming inspection, packaging, storage and safety

Verify AHEW, water content and viscosity on each lot against the COA. A shift in water content moves the applied solids and the coverage, and viscosity alone will not reveal it.

Drums carry at least 12 months of shelf life in unopened packing at ambient temperature, and the material must be kept from frost. The amine is alkaline and attacks skin and eyes, so the MSDS governs; check every figure here against the current TDS and COA.

8. Frequently Asked Questions

What is the difference between AHEW and amine value in a waterborne epoxy hardener?

AHEW is the mass of hardener carrying one reactive hydrogen, so it drives dosage. Amine value counts every titratable group, including the neutralised nitrogen. The two differ by 4% to 82%.

How is phr calculated for a waterborne epoxy hardener?

phr = 100 × AHEW ÷ EEW of the resin as supplied. At EEW 190, AHEW 120 returns 63 phr. Recalculate when the resin lot changes: a 15 g/eq shift in EEW moves phr by 5%.

Can a waterborne epoxy hardener be applied to damp concrete?

YLH-1003W is the grade the catalog lists for damp surfaces. A damp slab is not a wet one: standing water and laitance defeat any hardener.

Why does a waterborne epoxy film stay milky or tacky?

Milky means water is still in the film, from a thick coat or high humidity. Tacky usually means under-dosing from the amine value, or a carbonate bloom from CO2 attack.

Does a waterborne epoxy system reach zero VOC?

Not by construction. Water is excluded from the VOC figure in most jurisdictions, but the neutralising acid and any co-solvent count. Check the local definition before a tender.

Can a standard polyamide hardener be used in a waterborne epoxy?

Not directly. YLH-5022 is 95% solids and needs solvent to reach application viscosity. A polyamide can be emulsified, but that is a separate step.

9. Conclusions

Fourteen waterborne amine hardeners span AHEW 73-300 g/eq and phr 35-180. At a fixed 100 µm film the hardener mass moves 32 to 70 g/m2, a 2.2-fold spread the VOC figure does not show.

Amine value cannot substitute for AHEW: the neutralised nitrogen inflates the titration and the derived phr under-doses by 4% to 82%. Water carries nine times the evaporation energy of xylene per square metre, but dwell time, not money, is what the line feels.

10. References

1. Yolatech 2026 product catalog, waterborne amine section, page 14; TDS for each grade on request.

2. Yolatech product page: https://www.yolatech.com/solid-bisphenol-a-epoxy-resin (accessed 2026-11-27).

3. Yolatech product page: https://www.yolatech.com/hardener-ylh-5022 (accessed 2026-11-27).

4. ASTM D1652, epoxy content of epoxy resins (EEW).

5. ISO 3001, determination of epoxy equivalent.

6. ISO 9702, amine group nitrogen content of amine epoxide hardeners.

7. ASTM D445, kinematic viscosity.

dejar un mensaje

dejar un mensaje
Si está interesado en nuestros productos y desea conocer más detalles, deje un mensaje aquí, le responderemos lo antes posible.
Entregar

Hogar

Productos

Whatsapp

Contáctenos